HT PIPE whakarato Hastelloy C276 Nickel alloy porowhita pae, Alloy C276 Bar kaiwhakarato i Haina. 2.4819 pae porowhita, Alloy C276 tokotoko, UNS N10276 tokotoko, Alloy C276 Pae papatahi, Hastelloy C276 pae hollow, Hastelloy C276 Nickel alloy porowhita kaiwhakarato, kaihoko.

Hastelloy C-276 (3)

He aha nga ahuatanga o Hastelloy C276?

● He pai te aukati i te waikura ki te whakaiti i nga taiao
● He ātete tino pai ki nga otinga kaha o te tote waikura, penei i te ferric me te kapu puota.
● Ko nga ihirangi nickel me te molybdenum teitei e whakarato ana i te pai o te waikura ki te whakaiti i nga taiao
● He iti te waro o te waro e whakaiti ana i te rerenga carbide rohenga witi i te wa o te whakapiri kia mau tonu te atete ki te waikura i roto i nga rohe e pa ana ki te wera o nga hononga paiherea
● Te ātete ki te waikura o te rohe penei i te rua me te pakaru o te ahotea-waikura
● Ko tetahi o nga rawa iti hei tu ki nga paanga kino o te hau maota maku, hypochlorite me te chlorine dioxide

Hastelloy C276 Nickel alloy a tawhio pae Tito matū, %

Ni

Mo

Cr

Fe

W

Co

Mn

C

V

P

S

Si

Te toenga 15.0-17.0 14.5-16.5 4.0-7.0 3.0-4.5 2.5 te teitei 1.0 mōrahi .01 te teitei .35 te teitei .04 te teitei .03 te teitei .08 te teitei

Whakatakotoranga

Ko nga korero a te ASTM

Paipa Smls

Paipa paipa

Ngongo Smls

Tube Welded

Pepa/Pereti

Pae

Te patupatu

Whakapaipai

Waea

B622 B619 B622 B626 B575 B574 B564 B366  

Hastelloy C276 Āhuatanga ā-tinana

Ira whakarewa: 1325-1370 ℃

Kiato: 8.90 g/cm3

Alloy C276 Pae Mechanical Properties

Nga taonga miihini Tana, min, ksi[MPa] Hua, min, ksi[MPa] Whakaroa, %(min)
Hastelloy C276 100[690] 41[283] 40

Nga Ahuatanga Tensile Rūma Angamaheni o te Rauemi Anaa

Puka Hua

Maama (ksi)

.2% Hua (ksi)

Whakaroa %

Pae

110.0

52.6

62

Pereti

107.4

50.3

67

Rau

115.5

54.6

60

Ngongo & Paipa

105.4

45.4

70

Tikanga a te Kamupene

Te Tirohanga a te Kamupene: Tarapa me nga Taputapu Kanawete Waitohu Kairangi

Te Misioni a te Kamupene: I hangaia ma te whakaaro nui, Te kamupene whakamutunga, Hangaia he uara teitei ake mo nga kaihoko me te harikoa me nga kaimahi


  • Tōmua:
  • Panuku:

  • Tuhia to korero ki konei ka tukuna mai ki a matou