Korohanga Tino Tino
Te Whakamahana Teitei
◆1J50 he porowhita hysteresis porowhita me te waiwai nui autō induction.Ko te nuinga o te whakamahi i roto i nga whakakaha papa aukume, nga kowaowao coils, rectifier coils, me nga taputapu rorohiko e mahi ana i roto i nga mara autō reo.
◆1J79 he teitei te uruhanga autō tuatahi, a he pai mo nga momo hurihanga, hurihanga, whakakaha autō, kowaowao matua me nga whakangungu rakau e mahi ana i roto i nga mara autō ngoikore.
Ko te ◆3J53 he iti te waahi o te pāmahana i roto i te awhe o te -40-80 ° C, ka whakamahia mo te wiri i roto i te miihini miihini, te kakaho o te reera wiri me etahi atu waahanga.
◆4J29(F15) he whakarea roha waiariki raina rite ki tera o te karaehe pakeke i roto i tetahi awhe pāmahana, a ka whakamahia mo te whakataurite ki te karaihe pakeke i roto i te umanga korehau.
Ko te ◆4J36 he koranu rino-nickel iti-whakawhanui motuhake me te whakarea whakareatanga ultra-iti, e whakamahia ana i roto i te taiao e hiahia ana kia iti rawa te whakarea roha.
◆4J42 te nuinga whakamahia i roto i te hanga o ngā pūrere mārua hiko, taputapu pū, taputapu mataotao arorangi ki ngā whakaritenga pūmautanga tiketike, etc.
Te hanganga matū
Kōeke | C | Si | Mn | S | P | Cr | Ni | Mo | Cu | Fe | Al | Co | Ti |
kaua e nui ake i | |||||||||||||
1J50 | 0.03 | 0.15~0.3 | 0.3~0.6 | 0.02 | 0.02 | - | 49.5~50.5 | - | ≤0.2 | turanga | — | — | — |
1J79 | 0.03 | 0.3~0.5 | 0.6~1.1 | 0.02 | 0.02 | - | 78.5~80.5 | 3.8~4.1 | ≤0.2 | turanga | — | — | — |
3J53 | 0.05 | 0.8 | 0.8 | 0.02 | 0.02 | 5.2~5.8 | 41.5~43 | 0.7~0.9 | — | turanga | 0.5~0.8 | — | 2.3~2.7 |
4J29 | 0.03 | 0.3 | 0.5 | 0.02 | 0.02 | <0.2 | 28.5~29.5 | <0.2 | ≤0.2 | turanga | — | 16.8~17.8 | — |
4J36 | 0.05 | 0.3 | 0.2~0.6 | 0.02 | 0.02 | - | 35~37 | - | — | turanga | — | — | — |
4J42 | 0.05 | 0.3 | 0.8 | 0.02 | 0.02 | - | 41.5~42.5 | — | — | turanga | ≤0.1 | ≤1.0 | - |
Te iti rawa o nga rawa konumohe
Kōeke | Te momo | Ngā āhuatanga autō | ||
Te uruhanga tuatahi uo(MH/m) | Te Tiaki Morahi(Uh/m) | Te Whakaaetanga Hc(A/m) | ||
1J79 | Te takai makariri | ≥31 | ≥250 | ≤1.2 |
papa waea rakau | ≥25 | ≥125 | ≤2.4 | |
1J50 | Te takai makariri | ≥3.8 | ≥62.5 | ≤9.6 |
Paepae (whakatakahia). | ≥3.1 | ≥31.3 | ≤14.4 |
Kōeke | āhua | Kōwae Elastic E(Mpa) | te kaha mārō b(N/m㎡) | Te pakeke Hv |
3J53 | mahi makariri + pakeke | 190000~215600 | 1170~1760 | 400~480 |
Kōeke | Tauwaenga Raina Roha Whakarea (10-6℃) | ||||||
20~100℃ | 20~300℃ | 20~400℃ | 20~450℃ | 20~500℃ | 20~530℃ | 20~600℃ | |
4J29 | — | — | 4.6~5.2 | 5.1~5.5 | — | — | — |
4J50 | — | 9.2~10 | 9.2~9.9 | — | — | — | — |
4J36 | — | ≤1.5 | — | — | — | — | — |
4J42 | 5.5 | 4.6 | 5.8 | 6.7 | 7.6 | — | 9.1 |